Standard Practice for Preparation and Use of Direct Tension Stress-Corrosion Test Specimens
1.1 This practice covers procedures for designing, preparing, and using ASTM standard tension test specimens for investigating susceptibility to stress-corrosion cracking. Axially loaded specimens may be stressed quantitatively with equipment for application of either a constant load, constant strain, or with a continuously increasing strain.
1.2 Tension test specimens are adaptable for testing a wide variety of product forms as well as parts joined by welding, riveting, or various other methods.
1.3 The exposure of specimens in a corrosive environment is treated only briefly because other StandardDetails are being prepared to deal with this aspect. Meanwhile, the investigator is referred to Practices G 35, G 36, G 37, and G 44, and to ASTM Special Technical Publication 425