ISO 7539-12:2023

Corrosion of metals and alloys — Stress corrosion testing — Part 12: Requirements for atmospheric stress corrosion cracking testing

Standard Details

This document specifies the general requirements for designing and conducting tests to assess the susceptibility of metals and alloys to stress corrosion cracking under atmospheric exposure conditions.

The testing methodology includes exposure to natural environments and environments in artificially accelerated laboratory tests.

Applications include aluminium and its alloys in aerospace and construction; stainless steels in construction, pressure vessels, and nuclear waste containment; high strength low alloy steels in automotive, construction, and in lifting chains.

General Information

Status : Published
Standard Type: Main
Document No: ISO 7539-12:2023
Document Year: 2023
Pages: 11
Edition: 1
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals

Life Cycle

Currently Viewing

Published
ISO 7539-12:2023
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2025 BSB Edge Private Limited.

Enquire now +